3d Calcs
CONFIG:
130 W
$0.15/kWh
$20.00/kg spool
DENSITY: 1.24 g/cm³Not Required

Silk PLA (Gloss Finish)

PLA blended with elastomeric polymers for a metallic, high-sheen satin luster. Ideal for decorative display models.

Nozzle Temperature
210 - 230 °C
Extrusion hotend range
Bed Temperature
50 - 65 °C
PEI build plate setting
Drying Specs
45 °C
4 - 6 hours
1kg Spool Yield (1.75mm)
~335 meters
≈ 1100 feet

Silk PLA (Gloss Finish) Calculators

Silk PLA (Gloss Finish) (1.24 g/cm³)

Conversion Mode
grams
Filament Diameter
1.24 g/cm³
RESULTS & BREAKDOWNV=πr²L
Filament Length (m)
335.3meters
≈ 1100.0 feet (0.335 km)
Weight:1000.00 g (1.000 kg)
Linear Mass:2.98 g/meter
Total Volume:806.45 cm³
Cross-Section Area:2.405 mm²
Quick Rule of Thumb
Standard 1.75mm PLA yields approximately 330–335 meters per 1 kg spool. PETG yields ~327m, and ABS yields ~400m due to lower density.

Slicer Tuning & Cooling Profile

Part Cooling Fan
100%
Enclosure Requirement
Not Required
Polymer Specific Gravity
1.24 g/cm³

Silk PLA • Frequently Asked Questions

How many meters of filament are in a 1kg spool of Silk PLA?

A standard 1 kg spool of 1.75 mm Silk PLA filament yields approximately 335.3 meters (1100 feet) of printable material based on its polymer density of 1.24 g/cm³.

What nozzle and bed temperature should I use for Silk PLA?

Optimal extrusion temperature for Silk PLA is 210 - 230 °C with a heated bed temperature of 50 - 65 °C.

Does Silk PLA require an enclosed 3D printer or active ventilation?

Silk PLA enclosure status: Not Required. Polymers like ABS, ASA, and Nylon emit ultrafine particles (UFPs) and VOCs and warp easily from ambient air drafts, whereas PLA and PETG print safely in open-frame printers.

How do I dry Silk PLA filament and prevent moisture-related stringing?

Dry Silk PLA in a dedicated filament dryer or convection oven at 45 °C for 4 - 6 hours. Store with desiccant in vacuum-sealed bags to avoid steam popping, stringing, and brittle filament.

How do I prevent warping and get Silk PLA to stick to the build plate?

Clean the build plate thoroughly with warm water and grease-cutting dish soap (or 99% IPA). Set the part cooling fan to 100%, ensure first-layer squish is dialed in, and use a 5mm-8mm brim for tall or sharp-cornered models.